Reply to "Injuries associated to steel plate armor?"

MAC19D posted:

...There was a small dent in the plate, and a circle of the coating about 2 inches across blown away... 

While I have seen some legit rubbery coating with fibers under that look like spall coating inside armored vehicles, most plate coatings I see are like this. Often even come from the factory with corners chipped off. Unless I missed something about the material properties, spall shields seem like they should not be brittle.